Analysis of lignin and extractives in the oak wood of the 17th century warship Vasa
KTH, Skolan för kemivetenskap (CHE), Fiber- och polymerteknik, Träkemi och massateknologi.
KTH, Skolan för kemivetenskap (CHE), Fiber- och polymerteknik, Träkemi och massateknologi.
KTH, Skolan för kemivetenskap (CHE), Centra, Wallenberg Wood Science Center.
Vise andre og tillknytning
2014 (engelsk)Inngår i: Holzforschung, ISSN 0018-3830, E-ISSN 1437-434X, Vol. 68, nr 4, s. 419-425Artikkel i tidsskrift (Fagfellevurdert) Published
Abstract [en]

The wood in the 17th century Swedish warship Vasa is weak. A depolymerization of the wood's cellulose has been linked to the weakening, but the chemical mechanisms are yet unclear. The objective of this study was to analyze the lignin and tannin moieties of the wood to clarify whether the depolymerization of cellulose via ongoing oxidative mechanisms is indeed the main reason for weakening the wood in the Vasa. Lignin was analyzed by solid-state nuclear magnetic resonance [cross-polarization/magic-angle spinning (CP/MAS) C-13 NMR] and by means of wet chemical degradation (thioacidolysis) followed by gas chromatography-mass spectrometry (GC-MS) of the products. No differences could be observed between the Vasa samples and the reference samples that could have been ascribed to extensive lignin degradation. Wood extracts (tannins) were analyzed by matrix- assisted laser desorption ionization (MALDI) combined with time-of-flight (TOF) MS and C-13 NMR spectroscopy. The wood of the Vasa contained no discernible amounts of tannins, whereas still-waterlogged Vasa wood contained ellagic acid and traces of castalagin/vescalagin and grandinin. The results indicate that the condition of lignin in the Vasa wood is similar to fresh oak and that potentially harmful tannins are not present in high amounts. Thus, oxidative degradation mechanisms are not supported as a primary route to cellulose depolymerization.

sted, utgiver, år, opplag, sider
2014. Vol. 68, nr 4, s. 419-425
Emneord [en]
archeological wood, degradation, extraction, lignin, oak wood, oxidative degradation, tannins, thioacidolysis, Vasa
HSV kategori
Identifikatorer
URN: urn:nbn:se:kth:diva-146142DOI: 10.1515/hf-2013-0067ISI: 000335650900007Scopus ID: 2-s2.0-84899852871OAI: oai:DiVA.org:kth-146142DiVA, id: diva2:722721
Forskningsfinansiär
Swedish Research CouncilSwedish Foundation for Strategic Research FormasVinnova
Merknad

QC 20140609

Tilgjengelig fra: 2014-06-09 Laget: 2014-06-09 Sist oppdatert: 2017-12-05bibliografisk kontrollert

Open Access i DiVA

Fulltekst mangler i DiVA

Andre lenker

Forlagets fulltekstScopus

Søk i DiVA

Av forfatter/redaktør
Dedic, DinaSandberg, TeresiaIversen, TommyEk, Monica
Av organisasjonen
I samme tidsskrift
Holzforschung

Søk utenfor DiVA

GoogleGoogle Scholar

doi
urn-nbn

Altmetric

doi
urn-nbn
Totalt: 899 treff
RefereraExporteraLink to record
Permanent link

Direct link
Referera
Referensformat
  • apa
  • harvard1
  • ieee
  • modern-language-association-8th-edition
  • vancouver
  • Annet format
Fler format
Språk
  • de-DE
  • en-GB
  • en-US
  • fi-FI
  • nn-NO
  • nn-NB
  • sv-SE
  • Annet språk
Fler språk
Utmatningsformat
  • html
  • text
  • asciidoc
  • rtf