Reverse Magnetization Behavior Investigation of Mn-Al-C-(α-Fe) Nanocomposite Alloys with Different α-Fe Content Using First-Order Reversal Curves Analysis
Univ Tehran, Coll Engn, Sch Met & Mat, Adv Magnet Mat Res Ctr, Tehran 111554563, Iran..
Univ Tehran, Coll Engn, Sch Met & Mat, Adv Magnet Mat Res Ctr, Tehran 111554563, Iran..
Univ Tehran, Coll Engn, Sch Met & Mat, Adv Magnet Mat Res Ctr, Tehran 111554563, Iran..
KTH, Skolan för teknikvetenskap (SCI), Tillämpad fysik.ORCID-id: 0000-0002-5672-5727
2022 (Engelska)Ingår i: Nanomaterials, E-ISSN 2079-4991, Vol. 12, nr 19, s. 3303-, artikel-id 3303Artikel i tidskrift (Refereegranskat) Published
Abstract [en]

The reverse magnetization behavior for bulk composite alloys containing Mn-Al-C and α-Fe nanoparticles (NPs) has been investigated by hysteresis loops, recoil, and first-order reversal curves (FORC) analysis. The effect of adding different percentages of α-Fe (5, 10, 15, and 20 wt. %) on the magnetic properties and demagnetization behavior of Mn-Al-C nanostructured bulk magnets was investigated. The fabricated nanocomposites were characterized by XRD and VSM for structural analysis and magnetic behavior investigations, respectively. The demagnetization curve of the sample Mn-Al-C-5wt. % α-Fe showed a single hard magnetic behavior and showed the highest increase in remanence magnetization compared to the sample without α-Fe, and therefore this combination was selected as the optimal composition for FORC analysis. Magnetic properties for Mn-Al-C-5 wt. % α-Fe nanocomposite were obtained as Ms = 75 emu/g, Mr = 46 emu/g, Hc = 3.3 kOe, and (BH)max = 1.6 MGOe, indicating a much higher (BH)max than the sample with no α-Fe. FORC analysis was performed to identify exchange coupling for the Mn-Al-C-0.05α-Fe nanocomposite sample. The results of this analysis showed the presence of two soft and hard ferromagnetic components. Further, it showed that the reverse magnetization process in the composite sample containing 5 wt. % α-Fe is the domain rotation model.

Ort, förlag, år, upplaga, sidor
MDPI AG , 2022. Vol. 12, nr 19, s. 3303-, artikel-id 3303
Nyckelord [en]
reverse magnetization, recoil curve, FORC analysis, Henkel plot, MnAlC
Nationell ämneskategori
Metallurgi och metalliska material
Identifikatorer
URN: urn:nbn:se:kth:diva-320699DOI: 10.3390/nano12193303ISI: 000867047700001PubMedID: 36234431Scopus ID: 2-s2.0-85139770526OAI: oai:DiVA.org:kth-320699DiVA, id: diva2:1707196
Anmärkning

QC 20221031

Tillgänglig från: 2022-10-31 Skapad: 2022-10-31 Senast uppdaterad: 2022-10-31Bibliografiskt granskad

Open Access i DiVA

Fulltext saknas i DiVA

Övriga länkar

Förlagets fulltextPubMedScopus

Person

Hamawandi, Bejan

Sök vidare i DiVA

Av författaren/redaktören
Hamawandi, Bejan
Av organisationen
Tillämpad fysik
I samma tidskrift
Nanomaterials
Metallurgi och metalliska material

Sök vidare utanför DiVA

GoogleGoogle Scholar

doi
pubmed
urn-nbn

Altmetricpoäng

doi
pubmed
urn-nbn
Totalt: 16 träffar
RefereraExporteraLänk till posten
Permanent länk

Direktlänk
Referera
Referensformat
  • apa
  • ieee
  • modern-language-association-8th-edition
  • vancouver
  • Annat format
Fler format
Språk
  • de-DE
  • en-GB
  • en-US
  • fi-FI
  • nn-NO
  • nn-NB
  • sv-SE
  • Annat språk
Fler språk
Utmatningsformat
  • html
  • text
  • asciidoc
  • rtf