Application of tungsten for plasma limiters in TEXTOR
Visa övriga samt affilieringar
2000 (Engelska)Ingår i: Journal of Nuclear Materials, ISSN 0022-3115, E-ISSN 1873-4820, Vol. 283, s. 1128-1133Artikel i tidskrift (Refereegranskat) Published
Abstract [en]

Three different types of W limiters were exposed in the TEXTOR plasma and the response of the plasma and materials performance of the limiters were investigated. 1. A W bulk limiter operated with preheating above 800 K withstood a plasma heat load of about similar to 20 MW/m(2) for a few seconds with some slight surface melting during the highest heat load shot. However, it was severely damaged when operated at around 500 K. 2. A C/W twin test limiter, half made of bulk W and the other half of graphite (EK-98) gave very useful information on how low- and high-Z materials behave under conditions of simultaneous utilization as PFM such as cross-contamination and the influence of a large mass difference on hydrogen reflection and deposition. 3. Two sets of main poloidal W limiters made of vacuum vapor sprayed (VPS)-W deposited on graphite (IG-430U) with a Re interlayer could absorb about 60% of the total convection heat and the ohmic plasma with a density as high as 5 x 10(13) cm(-3) was sustained. Most of the VPS-W coated limiters tolerated a heal load of similar to 20 MW/m(2). This series of W limiters experiments in TEXTOR has shown that W is applicable as a PFM, if its central accumulation is avoided by NBI and/or ICRH heating. Nevertheless, some concerns still remain, including difficulty of plasma startup, W behavior in higher temperature plasmas, and materials' selection.

Ort, förlag, år, upplaga, sidor
2000. Vol. 283, s. 1128-1133
Nyckelord [en]
edge
Identifikatorer
URN: urn:nbn:se:kth:diva-20229DOI: 10.1016/S0022-3115(00)00119-7ISI: 000165877800081OAI: oai:DiVA.org:kth-20229DiVA, id: diva2:338922
Anmärkning
QC 20100525Tillgänglig från: 2010-08-10 Skapad: 2010-08-10 Senast uppdaterad: 2017-12-12Bibliografiskt granskad

Open Access i DiVA

Fulltext saknas i DiVA

Övriga länkar

Förlagets fulltext

Personposter BETA

Rubel, Marek J.

Sök vidare i DiVA

Av författaren/redaktören
Rubel, Marek J.
Av organisationen
Alfvénlaboratoriet
I samma tidskrift
Journal of Nuclear Materials

Sök vidare utanför DiVA

GoogleGoogle Scholar

doi
urn-nbn

Altmetricpoäng

doi
urn-nbn
Totalt: 48 träffar
RefereraExporteraLänk till posten
Permanent länk

Direktlänk
Referera
Referensformat
  • apa
  • ieee
  • modern-language-association-8th-edition
  • vancouver
  • Annat format
Fler format
Språk
  • de-DE
  • en-GB
  • en-US
  • fi-FI
  • nn-NO
  • nn-NB
  • sv-SE
  • Annat språk
Fler språk
Utmatningsformat
  • html
  • text
  • asciidoc
  • rtf