Hydrogen depth profile in phosphorus-doped, oxygen-free copper after cathodic charging
KTH, Skolan för industriell teknik och management (ITM), Materialvetenskap, Materialteknologi.ORCID-id: 0000-0002-8494-3983
2012 (Engelska)Ingår i: Journal of Materials Science, ISSN 0022-2461, E-ISSN 1573-4803, Vol. 47, nr 19, s. 6768-6776Artikel i tidskrift (Refereegranskat) Published
Abstract [en]

Spent nuclear fuel, in Sweden, is planned to be put in 50-mm thick copper canisters and placed in 500-m depth in the bedrock. Depending on the conditions in the repository, an uptake of hydrogen in the copper may occur. It is therefore necessary to establish how a hydrogen uptake affects the microstructure in both the surface and the bulk. Phosphorus-doped, oxygen-free copper has been cathodically charged with hydrogen for up to 3 weeks. The amount of hydrogen as a function of the distance from the surface was measured by two methods: glow discharge optical emission spectrometry and melt extraction. The penetration of the increased hydrogen content was about 50 mu m. Extensive bubble formation took place during the charging. A model has been formulated for the diffusion of hydrogen into the copper, the bubble formation and growth. The model can describe the total amount of hydrogen, the number of bubbles and their sizes as a function of the distance from the surface. Bubbles close to the surface caused the surface to bulge due to the high hydrogen pressure. From the shape of the deformed surface, the maximum hydrogen pressure could be estimated with the help of stress analysis. The maximum pressure was found to be about 400 MPa, which is almost an order of magnitude larger than previously recorded values for electroless deposited copper.

Ort, förlag, år, upplaga, sidor
2012. Vol. 47, nr 19, s. 6768-6776
Nyckelord [en]
Electroless Copper, Ductility, Deposits, Bubbles, Diffusivity, Silver, Creep, Gold, Cu
Nationell ämneskategori
Materialteknik
Identifikatorer
URN: urn:nbn:se:kth:diva-100773DOI: 10.1007/s10853-012-6592-yISI: 000306436600002Scopus ID: 2-s2.0-84864767427OAI: oai:DiVA.org:kth-100773DiVA, id: diva2:545006
Anmärkning
QC 20120817Tillgänglig från: 2012-08-17 Skapad: 2012-08-17 Senast uppdaterad: 2017-12-07Bibliografiskt granskad

Open Access i DiVA

Fulltext saknas i DiVA

Övriga länkar

Förlagets fulltextScopus

Personposter BETA

Sandström, Rolf

Sök vidare i DiVA

Av författaren/redaktören
Sandström, Rolf
Av organisationen
Materialteknologi
I samma tidskrift
Journal of Materials Science
Materialteknik

Sök vidare utanför DiVA

GoogleGoogle Scholar

doi
urn-nbn

Altmetricpoäng

doi
urn-nbn
Totalt: 350 träffar
RefereraExporteraLänk till posten
Permanent länk

Direktlänk
Referera
Referensformat
  • apa
  • harvard1
  • ieee
  • modern-language-association-8th-edition
  • vancouver
  • Annat format
Fler format
Språk
  • de-DE
  • en-GB
  • en-US
  • fi-FI
  • nn-NO
  • nn-NB
  • sv-SE
  • Annat språk
Fler språk
Utmatningsformat
  • html
  • text
  • asciidoc
  • rtf