Corrosion-induced release of chromium and iron from ferritic stainless steel grade AISI 430 in simulated food contact
KTH, Skolan för kemivetenskap (CHE), Kemi, Korrosionslära.ORCID-id: 0000-0002-2123-2201
KTH, Skolan för kemivetenskap (CHE), Kemi, Korrosionslära.ORCID-id: 0000-0003-2206-0082
KTH, Skolan för kemivetenskap (CHE), Kemi, Korrosionslära.ORCID-id: 0000-0002-9453-1333
2008 (Engelska)Ingår i: Journal of Food Engineering, ISSN 0260-8774, E-ISSN 1873-5770, Vol. 87, nr 2, s. 291-300Artikel i tidskrift (Refereegranskat) Published
Abstract [en]

Ferritic stainless steel grade AISI 430 with three different surface finishes, glossy, line and abraded has been evaluated regarding changes in metal release rates and corresponding changes in surface composition when immersed in 3 vol% acetic acid at two different temperatures, 40 degrees C for ten days and 100 degrees C during three consecutive immersions of 30 min each. Test parameter intervals were set by one of the very few regulatory texts for metal release in food applications, the Italian law text D.M. 21-03-1973, Art. 37. The metal release process was found to be strongly dependent on surface area to solution volume ratio where a specific surface finish would be within the allowed limit, 0.1 mg Cr L-1 for the lowest ratio, 0.5 cm, but exceeded for the highest ratio, 2 cm(-1). The amount of released metal increased with increasing temperature and increasing surface roughness (surface finish).

Generated data show the regulatory text insufficient and to provide large degrees of freedom, specifically in terms of defining the surface area to solution volume ratio and the acidic cleaning of test vessels, essential parameters to enable reproducible and relevant migration data.

Ort, förlag, år, upplaga, sidor
2008. Vol. 87, nr 2, s. 291-300
Nyckelord [en]
metal release; acetic acid; ferritic stainless steel; iron; chromium; cuttlery
Nationell ämneskategori
Teknik och teknologier
Identifikatorer
URN: urn:nbn:se:kth:diva-8527DOI: 10.1016/j.jfoodeng.2007.12.006ISI: 000254722500016Scopus ID: 2-s2.0-39749135591OAI: oai:DiVA.org:kth-8527DiVA, id: diva2:13875
Anmärkning
QC 20100810Tillgänglig från: 2008-05-27 Skapad: 2008-05-27 Senast uppdaterad: 2017-12-14Bibliografiskt granskad
Ingår i avhandling
1. Bioaccessibility of Stainless Steels: Importance of Bulk and Surface Features
Öppna denna publikation i ny flik eller fönster >>Bioaccessibility of Stainless Steels: Importance of Bulk and Surface Features
2008 (Engelska)Doktorsavhandling, sammanläggning (Övrigt vetenskapligt)
Abstract [en]

With increasing environmental awareness, the desire to protect human beings and the environment from adverse effects induced by dispersed metals has become an issue of great concern and interest. New policies, such as REACH (Registration, Evaluation, Authorisation and Restriction of Chemicals) within the European Community, have been implemented to reduce hazards posed by the use of chemicals on producers and downstream users. The generation of exposure assessment data and relevant test procedures able to simulate realistic scenarios are essential in such legislative actions.

This doctoral study was initiated to fill knowledge gaps related to the metal release process of stainless steels. A wide range of stainless steel grades, fourteen in total, were investigated. They cover a very broad range of applications, and the focus in the thesis was to simulate a few selected exposure scenarios: precipitation, the human body and food intake. Comparisons were made between metal release from stainless steel alloys and the pure metals that constitute each stainless steel in order to explore the differences between alloys and pure metals, and to provide quantitative data on metal release rates of different alloy constituents. Because of similar surface properties between stainless steel and pure chromium, this metal exhibits similar release rates, whereas iron and nickel exhibit significantly lower release rates as alloy components than as pure metals. Detailed studies were also performed to elucidate possible relations between metal release and steel surface properties. Key parameters turned out to be chromium enrichment of the self-passivating surface film, surface roughness, the electrochemically active surface area and the microstructure of the steel substrate. The degree of metal release increased with decreasing chromium content in the surface oxide, increasing surface roughness, and increasing presence of inhomogeneities in the bulk matrix.

More detailed studies were initiated to possibly correlate the nucleation of metastable pits and the extent of metal release. Evidence was given that metastable pits exist even when the stainless steel is passive, and may cause extremely short-lived bursts of released metal before the surface film repassivates again.

Ort, förlag, år, upplaga, sidor
Stockholm: KTH, 2008. s. 73
Serie
Trita-CHE-Report, ISSN 1654-1081 ; 2008:39
Nyckelord
Stainless steel, iron, chromium, nickel, corrosion, metal release, artificial rain, synthetic body fluids, acetic acid, surface oxide, surface finish
Nationell ämneskategori
Fysikalisk kemi
Identifikatorer
urn:nbn:se:kth:diva-4773 (URN)978-91-7178-977-8 (ISBN)
Disputation
2008-06-03, F3, KTH, Lindstedtsvägen 26, Stockholm, 10:00
Opponent
Handledare
Anmärkning
QC 20100810Tillgänglig från: 2008-05-27 Skapad: 2008-05-27 Senast uppdaterad: 2010-08-10Bibliografiskt granskad

Open Access i DiVA

Fulltext saknas i DiVA

Övriga länkar

Förlagets fulltextScopus

Personposter BETA

Herting, GunillaOdnevall Wallinder, IngerLeygraf, Christofer

Sök vidare i DiVA

Av författaren/redaktören
Herting, GunillaOdnevall Wallinder, IngerLeygraf, Christofer
Av organisationen
Korrosionslära
I samma tidskrift
Journal of Food Engineering
Teknik och teknologier

Sök vidare utanför DiVA

GoogleGoogle Scholar

doi
urn-nbn

Altmetricpoäng

doi
urn-nbn
Totalt: 140 träffar
RefereraExporteraLänk till posten
Permanent länk

Direktlänk
Referera
Referensformat
  • apa
  • ieee
  • modern-language-association-8th-edition
  • vancouver
  • Annat format
Fler format
Språk
  • de-DE
  • en-GB
  • en-US
  • fi-FI
  • nn-NO
  • nn-NB
  • sv-SE
  • Annat språk
Fler språk
Utmatningsformat
  • html
  • text
  • asciidoc
  • rtf