Contact corrosion resistance between the cathode and current collector plate in the molten carbonate fuel cell
KTH, Tidigare Institutioner                               , Kemiteknik.ORCID-id: 0000-0002-2268-5042
KTH, Tidigare Institutioner                               , Kemiteknik.ORCID-id: 0000-0001-9203-9313
Vise andre og tillknytning
2001 (engelsk)Inngår i: Journal of the Electrochemical Society, ISSN 0013-4651, E-ISSN 1945-7111, Vol. 148, nr 1, s. A38-A43Artikkel i tidsskrift (Fagfellevurdert) Published
Abstract [en]

The corrosion layer Formed in the contact between the cathode and the current collector is one factor limiting the cathode performance in molten carbonate fuel cells (MCFC). In order to investigate the contribution to the total polarization of the contact resistance, electrochemical experiments were performed in a laboratory-scale fuel cell unit with a specially designed current collector. Two cathode materials, NiO and LiCoO2, were investigated to elucidate the impact of the cathode material on the formed corrosion layer. Polarization measurements as well as electrochemical impedance spectroscopy were used. The method works well for NiO electrodes. However, due to the poor electronic conductivity in the LiCoO2 electrode, the experimental results become difficult to evaluate due to a nonuniform potential distribution. The contact resistance between the cathode and the current collector contributes with a large value to the total cathode polarization. The corrosion layer in case of the LiCoO2 cathode was iron-rich and has a thickness of about 20 mum after 8 weeks operation of the fuel cell. Ln the case of the NiO cathode, a nickel-rich corrosion layer of about 15 mum was formed after 5 weeks operation of the fuel cell.

sted, utgiver, år, opplag, sider
2001. Vol. 148, nr 1, s. A38-A43
Emneord [en]
surface characterization methods, nickel-oxide, base alloys, performance, electrodes, behavior, polarization, alkali
Identifikatorer
URN: urn:nbn:se:kth:diva-20258ISI: 000166129600006OAI: oai:DiVA.org:kth-20258DiVA, id: diva2:338951
Merknad
QC 20100525Tilgjengelig fra: 2010-08-10 Laget: 2010-08-10 Sist oppdatert: 2017-12-12bibliografisk kontrollert

Open Access i DiVA

Fulltekst mangler i DiVA

Personposter BETA

Lagergren, CarinaLindbergh, Göran

Søk i DiVA

Av forfatter/redaktør
Lagergren, CarinaLindbergh, Göran
Av organisasjonen
I samme tidsskrift
Journal of the Electrochemical Society

Søk utenfor DiVA

GoogleGoogle Scholar

urn-nbn

Altmetric

urn-nbn
Totalt: 240 treff
RefereraExporteraLink to record
Permanent link

Direct link
Referera
Referensformat
  • apa
  • ieee
  • modern-language-association-8th-edition
  • vancouver
  • Annet format
Fler format
Språk
  • de-DE
  • en-GB
  • en-US
  • fi-FI
  • nn-NO
  • nn-NB
  • sv-SE
  • Annet språk
Fler språk
Utmatningsformat
  • html
  • text
  • asciidoc
  • rtf