Material valorisation of amorphous polylactide. Influence of thermo-mechanical degradation on the morphology, segmental dynamics, thermal and mechanical performance
KTH, Skolan för kemivetenskap (CHE), Fiber- och polymerteknik, Polymera material.ORCID-id: 0000-0002-2139-7460
KTH, Skolan för kemivetenskap (CHE), Fiber- och polymerteknik, Polymera material.ORCID-id: 0000-0002-5394-7850
2012 (engelsk)Inngår i: Polymer degradation and stability, ISSN 0141-3910, E-ISSN 1873-2321, Vol. 97, nr 4, s. 670-678Artikkel i tidsskrift (Fagfellevurdert) Published
Abstract [en]

This paper reports the effects of multiple mechanical recycling on the structure and properties of amorphous polylactide (PIA). The influence of the thermo-mechanical degradation induced by means of five successive injection cycles was initially addressed in terms of macroscopic mechanical properties and surface modification. A deeper inspection on the structure and morphology of PLA was associated to the thermal properties and viscoelastic behaviour. Although FT-IR analysis did not show significant changes in functional groups, a remarkable reduction in molar mass was found by viscometry. PIA remained amorphous throughout the reprocessing cycles, but the occurrence of a cold-crystallization during DSC and DMTA measurements, which enthalpy increased with each reprocessing step, suggested chain scission due to thermo-mechanical degradation. The effect of chain shortening on the glass-rubber relaxation studied by DMTA showed an increase in free volume affecting the segmental dynamics of PLA, particularly after the application of the second reprocessing step, in connection to the overall loss of performance showed by the remaining properties.

sted, utgiver, år, opplag, sider
2012. Vol. 97, nr 4, s. 670-678
Emneord [en]
Polylactide (PLA), Material valorisation, Mechanical recycling, Thermo-mechanical degradation, Cold-crystallization, Segmental dynamics
HSV kategori
Identifikatorer
URN: urn:nbn:se:kth:diva-81465DOI: 10.1016/j.polymdegradstab.2011.12.019ISI: 000301911300027Scopus ID: 2-s2.0-84857632341OAI: oai:DiVA.org:kth-81465DiVA, id: diva2:497502
Merknad
QC 20120423Tilgjengelig fra: 2012-02-10 Laget: 2012-02-10 Sist oppdatert: 2017-12-07bibliografisk kontrollert

Open Access i DiVA

Fulltekst mangler i DiVA

Andre lenker

Forlagets fulltekstScopus

Personposter BETA

Strömberg, EmmaKarlsson, Sigbritt

Søk i DiVA

Av forfatter/redaktør
Strömberg, EmmaKarlsson, Sigbritt
Av organisasjonen
I samme tidsskrift
Polymer degradation and stability

Søk utenfor DiVA

GoogleGoogle Scholar

doi
urn-nbn

Altmetric

doi
urn-nbn
Totalt: 673 treff
RefereraExporteraLink to record
Permanent link

Direct link
Referera
Referensformat
  • apa
  • ieee
  • modern-language-association-8th-edition
  • vancouver
  • Annet format
Fler format
Språk
  • de-DE
  • en-GB
  • en-US
  • fi-FI
  • nn-NO
  • nn-NB
  • sv-SE
  • Annet språk
Fler språk
Utmatningsformat
  • html
  • text
  • asciidoc
  • rtf