Utmatningsformat
  • html
  • text
  • asciidoc
  • rtf
Superior mechanical performance of highly porous, anisotropic nanocellulose-montmorillonite aerogels prepared by freeze casting
KTH, Skolan för kemivetenskap (CHE), Centra, Wallenberg Wood Science Center.
KTH, Skolan för kemivetenskap (CHE), Fiber- och polymerteknologi, Biokompositer. KTH, Skolan för kemivetenskap (CHE), Centra, Wallenberg Wood Science Center.ORCID-id: 0000-0001-5818-2378
2014 (engelsk)Inngår i: Journal of The Mechanical Behavior of Biomedical Materials, ISSN 1751-6161, E-ISSN 1878-0180, Vol. 37, s. 88-99Artikkel i tidsskrift (Fagfellevurdert) Published
Abstract [en]

Directionally solidified nanofibrillated cellulose (NFC)-sodium-montmorillonite (MMT) composite aerogels with a honeycomb-like pore structure were compared with non-directionally frozen aerogels with equiaxed pore structure and identical composition and found to have superior functionalities. To explore structure-property correlations, three different aerogel compositions of 3 wt% MMT, and 0.4 wt%, 0.8 wt%, and 1.2 wt% NFC, respectively, were tested. Young's modulus, compressive strength and toughness were found to increase with increasing NFC content for both architectures. The modulus increased from 25.8 kPa to 386 kPa for the isotropic and from 2,13 MPa to 3.86 MPa for the anisotropic aerogels, the compressive yield strength increased from 3.3 kPa to 18.0 kPa for the isotropic and from 32.3 kPa to 52.5 kPa for the anisotropic aerogels, and the toughness increased from 6.3 kJ/m(3) to 24.1 kJ/m(3) for the isotropic and from 22.9 kJ/m(3) to 46.2 kJ/m(3) for the anisotropic aerogels. The great range of properties, which can be achieved through compositional as well as architectural variations, makes these aerogels highly attractive for a large range of applications, for which either a specific composition, or a particular pore morphology, or both are required. Finally, because NFC is flammable, gasification experiments were performed, which revealed that the inclusion of MMT increased the heat endurance and shape retention functions of the aerogels dramatically up to 800 degrees C while the mechanical properties were retained up to 300 degrees C.

sted, utgiver, år, opplag, sider
2014. Vol. 37, s. 88-99
Emneord [en]
Directional solidification, Honeycombs, Foams, Structure-property correlations, Nanoclay
HSV kategori
Identifikatorer
URN: urn:nbn:se:kth:diva-151330DOI: 10.1016/j.jmbbm.2014.05.012ISI: 000340987100010PubMedID: 24905177Scopus ID: 2-s2.0-84901788700OAI: oai:DiVA.org:kth-151330DiVA, id: diva2:748074
Merknad

QC 20140918

Tilgjengelig fra: 2014-09-18 Laget: 2014-09-18 Sist oppdatert: 2022-06-23bibliografisk kontrollert

Open Access i DiVA

Fulltekst mangler i DiVA

Andre lenker

Forlagets fulltekstPubMedScopus

Person

Berglund, Lars A.

Søk i DiVA

Av forfatter/redaktør
Liu, AndongBerglund, Lars A.
Av organisasjonen
I samme tidsskrift
Journal of The Mechanical Behavior of Biomedical Materials

Søk utenfor DiVA

GoogleGoogle Scholar

doi
pubmed
urn-nbn

Altmetric

doi
pubmed
urn-nbn
Totalt: 510 treff
RefereraExporteraLink to record
Permanent link

Direct link
Referera
Referensformat
  • apa
  • ieee
  • modern-language-association-8th-edition
  • vancouver
  • Annet format
Fler format
Språk
  • de-DE
  • en-GB
  • en-US
  • fi-FI
  • nn-NO
  • nn-NB
  • sv-SE
  • Annet språk
Fler språk
Utmatningsformat
  • html
  • text
  • asciidoc
  • rtf