Effect of Thermomechanical Treatment of Al-Zn-Mg-Cu with Minor Amount of Sc and Zr on the Mechanical Properties
Islamic Azad Univ, Shahrekord Branch, Dept Mech Engn, Shahrekord 8813733395, Iran..
Islamic Azad Univ, Sci & Res Branch, Dept Mat Engn, Tehran 8244865179, Iran..
Islamic Azad Univ, Shahrekord Branch, Young Researchers & Elite Club, Shahrekord 8813733395, Iran..
KTH, Skolan för teknikvetenskap (SCI), Tillämpad fysik, Biomedicinsk fysik och röntgenfysik.ORCID-id: 0000-0002-5672-5727
2022 (engelsk)Inngår i: Materials, E-ISSN 1996-1944, Vol. 15, nr 2, artikkel-id 589Artikkel i tidsskrift (Fagfellevurdert) Published
Abstract [en]

In this study, the mechanical and microstructural properties of Al-Zn-Mg-Cu-Zr cast alloy with 0.1% Sc under homogeneous, dissolution, and T6 and thermomechanical treatments with the aim of increasing the volume fraction of MgZn2. Al-3(Sc,Zr) reinforcing precipitates were examined by hardness, microscopic examinations, tensile tests and software analysis. The results showed that, firstly, the hardness results are well proportional to the results of the tensile properties of alloys and, secondly, the strength of the alloy with thermomechanical treatments compared to T6 treatments increased from 492 MPa to 620 MPa and the elongation increased from 8% to 17% and was 100% upgraded. Microstructural and fracture cross section investigations showed that Al-3(Sc,Zr) nanosize dispersoids were evenly distributed among MgZn2 dispersoids and the alloy fracture was of semi-ductile type and nanosize dispersoids less than 10 nm were observed at the end of the dimples in the fracture section. The volume fraction of nanosize dispersoids in the whole microstructure of thermomechanical treatment samples was also much higher than that of T6 heat treated samples, so that the percentage of Al-3(Sc,Zr) precipitates arrived from less than 1% in T6 operation to 8.28% in the quench-controlled thermomechanical operation (with 50% deformation). The quality index (QI) in thermomechanical treatment samples is 19% higher than T6 samples, so that this index has increased from 641 in T6 operation to 760 in samples under thermomechanical treatment due to precipitate morphology, volume fraction of precipitates, their uniform distribution in the matrix, and nano sized precipitates in samples under thermomechanical treatment.

sted, utgiver, år, opplag, sider
MDPI , 2022. Vol. 15, nr 2, artikkel-id 589
Emneord [en]
scandium, thermomechanical treatment, microstructure, 7000 series alloy
HSV kategori
Identifikatorer
URN: urn:nbn:se:kth:diva-308573DOI: 10.3390/ma15020589ISI: 000746416100001PubMedID: 35057304Scopus ID: 2-s2.0-85122980657OAI: oai:DiVA.org:kth-308573DiVA, id: diva2:1636670
Merknad

QC 20220210

Tilgjengelig fra: 2022-02-10 Laget: 2022-02-10 Sist oppdatert: 2024-07-04bibliografisk kontrollert

Open Access i DiVA

Fulltekst mangler i DiVA

Andre lenker

Forlagets fulltekstPubMedScopus

Person

Hamawandi, Bejan

Søk i DiVA

Av forfatter/redaktør
Hamawandi, Bejan
Av organisasjonen
I samme tidsskrift
Materials

Søk utenfor DiVA

GoogleGoogle Scholar

doi
pubmed
urn-nbn

Altmetric

doi
pubmed
urn-nbn
Totalt: 81 treff
RefereraExporteraLink to record
Permanent link

Direct link
Referera
Referensformat
  • apa
  • ieee
  • modern-language-association-8th-edition
  • vancouver
  • Annet format
Fler format
Språk
  • de-DE
  • en-GB
  • en-US
  • fi-FI
  • nn-NO
  • nn-NB
  • sv-SE
  • Annet språk
Fler språk
Utmatningsformat
  • html
  • text
  • asciidoc
  • rtf